Print this page

ATOM ARC 7018

Atom Arc 7018 was introduced in the United States in 1952 and continues to set the standard by which all other covered electrodes are judged. This low hydrogen, moisture resistant electrode is known throughout the world for its superior welding performance, tough mechanical properties, crack resistance, high operator appeal and consistent quality.

Features

Atom Arc 7018 is an all-position low hydrogen moisture resistant electrode. The wider operating ranges and smooth weld metal transfer minimizes post weld clean up. This premium quality electrode meets a multitude of codes and welding specifications. Atom Arc 7018 was developed to weld carbon and low-alloy steels, including a variety of hardenable steels.

ATOM ARC 7018
  • Industry
  • Shipbuilding
  • Mobile Machinery
  • Civil Construction
  • General Fabrication
  • Bridge Construction
  • Rail Road Car
  • Automotive
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • Mil-E-22200/1 Mil-7018
    • AWS A5.1; E7018H4R
    • A.B.S.- 2Y / AWS A5.1; E7018
    • D.N.V.- 3Y(H10)
    • ASME SFA 5.1
    • L.R.- 3m,3Ym(H10)
    • CERTIFIED BY C.W.B.- CSA W48

Properties

Typical Properties
As Welded  
Yield Strength 68 ksi, 470 MPa
Tensile Strength 78 ksi, 540 MPa
Elongation in 2" 30 %
Reduction in Area 75 %
Stress Relieved 8 hrs. @ 1150ºF (621ºC)  
Yield Strength 57 ksi, 395 MPa
Tensile Strength 70 ksi, 485 MPa
Reduction in Area 77 %
Elongation in 2" 33 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 168 ft.-lbs., 225 J
Stress Relieved 8 hrs. @ 1150ºF (621ºC) 193 ft.-lbs., 260 J
Typical Undiluted Weld Metal Analysis  
C 0.045 %
Mn 1.1 %
Si 0.4 %
P 0.015 %
S 0.014 %

SAW

Accessories

Depositions

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 90 A 70 - 100 1.7 lbs./hr., 0.8 kg./hr. 66.3 %
1/8 in, 3.2 mm 120 A 90 - 160 2.6 lbs./hr., 1.2 kg./hr. 71.6 %
140 A 90 - 160 2.7 lbs./hr., 1.2 kg./hr. 70.9 %
5/32 in, 4.0 mm 140 A 130 - 220 3.1 lbs./hr., 1.4 kg./hr. 75 %
170 A 130 - 220 3.8 lbs./hr., 1.7 kg./hr. 73.5 %
3/16 in, 4.8 mm 200 A 200 - 300 4.9 lbs./hr., 2.2 kg./hr. 76.4 %
250 A 200 - 300 5.4 lbs./hr., 2.4 kg./hr. 74.6 %
7/32 in, 5.6 mm 250 A 250 - 350 6.5 lbs./hr., 2.9 kg./hr. 75 %
300 A 250 - 350 7.2 lbs./hr., 3.3 kg./hr. 74 %
1/4 in, 6.4 mm 300 A 300 - 400 7.7 lbs./hr., 3.5 kg./hr. 78 %
350 A 300 - 400 8.7 lbs./hr., 3.9 kg./hr. 77 %

Extra Info