ARCALOY 308L-17 Plus

Arcaloy 308L Plus electrode utilize a heavy coating to maximize performance in the flat and horizontal position.

Features

Arcaloy 308L-17 Plus electrodes have a heavy coating, produce a concave bead with minimum ripple and the slag is virtually self-cleaning. These electrodes are designed to weld Types 304, 304L, 321 and 347 for corrosion service at temperature up to about 600ºF(315ºC).
The excellent wetting action and very fine ripple minimize crevice corrosion and grinding time. This is particularly useful in the food and drink industry where a smooth polished surface is required.

* This item is subject to Industry Alloy Surcharges

Arcaloy Plus 308L-17
  • Industry
  • Rail Road Car
  • Process
  • General Fabrication
  • Food and Beverage
  • Shipbuilding
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.4; E308-17/E308L-17
    • ASME IX F No. 5
    • ASME II SFA 5.4 E308-17/E308L-17

Properties

Typical Properties
Tensile Strength 86 ksi, 550 - 620 MPa
Elongation in 2" 47 %
Typical Undiluted Weld Metal Analysis  
C 0.02 %
Mn 0.6 %
Si 0.8 %
Cr 19 %
Ni 10 %
Mo 0.1 %
Cu 0.1 %
Ferrite 6 FN

SAW

Accessories

Depositions

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 205-290 mm

Extra Info

Arcaloy 308L-17 Plus electrodes are designed to produce a concave bead with minimum ripple and the slag is virtually self-releasing. This is particularly useful in the food and drink industry where a smooth polished surface is required. These electrodes are designed to weld Types 304, 304L, 321 and 347 for corrosion service at temperature up to about 600ºF(315ºC).