Print this page

OK Tigrod ER2509

OK Tigrod 2509 is a super duplex grade for high resistance to intergranular corrosion and pitting. The alloy is widely used in applications in which corrosion resistance is of the utmost importance. Can be used in combination with OK Flux 10.94.

Features

A solid, corrosion-resistant ''Super Duplex'' rod for the GTAW welding of austenitic-ferritic stainless alloys of the 25% Cr, 10% Ni, 4% Mo, low C types. OK Tigrod 2509 (''Super Duplex'') has high resistance to intergranular corrosion and pitting. The alloy is widely used in applications in which corrosion resistance is of the utmost importance.
The pulp and paper, offshore and gas industries are areas of interest.
OK Tigrod 2509 is also a submerged arc 25Cr10Ni4Mo type wire with extra-low carbon content for welding austenitic-ferritic, super-duplex stainless steels. OK Tigrod 2509 can be used in combination with OK Flux 10.94 or OK Flux 10.93.

* This item is subject to Industry Alloy Surcharges

Classifications

Properties

Typical Properties
Yield Strength 670 MPa
Tensile Strength 850 MPa
Elongation in 2" 30 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -40ºF (-40ºC) 115 J
Testing Temperature 68ºF (20ºC) 150 J
Typical Undiluted Weld Metal Analysis  
C <0.03 %
Mn <2.5 %
Si <1.0 %
Cr 25.5 %
Ni 9.2 %
Mo 3.5 %
N 0.25 %
Ferrite 30-50 FN

SAW

Accessories

Depositions

Extra Info