OK Flux 10.72 is a neutral, bonded aluminate-basic flux.
OK Flux 10.72 is a neutral, bonded aluminate-basic flux. It is primarily used for for applications with toughness requirements down to -50°C in high dilution joints. It provides excellent slag removal also in narrow V-joints. It is recommended for joining structural steels, fine grained steels and creep resistant steels. It has proved to be especially appropriate for wind tower productions. OK Flux 10.72 features extremely high current carrying capacity and is intended for single or multi wire procedures using DC and AC power. It can be used for single layer and multi layer welding of unlimited plate thickness.

| Typical Mechanical Properties | |
|---|---|
| As Welded | |
| Spoolarc 81 | |
| Tensile Strength | 75 ksi, 515 MPa |
| Yield Strength | 62 ksi, 425 MPa |
| Elongation in 2" | 30 % |
| CVN | 35 ft.-lbs., 50 J |
| Temperature | -80 °F, -62 °C |
| Spoolarc 75 | |
| Tensile Strength | 89 ksi, 655 MPa |
| Yield Strength | 76 ksi, 550 MPa |
| Elongation in 2" | 28 % |
| CVN | 110 ft.-lbs., 149 J |
| Temperature | -40 °F, -40 °C |
| Spoolarc ENi4 | |
| Tensile Strength | 96 ksi, 680 MPa |
| Yield Strength | 85 ksi, 585 MPa |
| Elongation in 2" | 26 % |
| CVN | 115 ft.-lbs., 156 J |
| Temperature | -40 °F, -40 °C |
| Stress Relieved 1 hr. @ 1150°F | |
| Spoolarc 81 | |
| Tensile Strength | 74 ksi, 510 MPa |
| Yield Strength | 59 ksi, 405 MPa |
| Elongation in 2" | 32 % |
| CVN | 35 ft.-lbs., 50 J |
| Temperature | -80 °F, -62 °C |
| Stress Relieved 8 hrs. @ 1150°F | |
| Spoolarc 81 | |
| Tensile Strength | 74 ksi, 510 MPa |
| Yield Strength | 58 ksi, 400 MPa |
| Elongation in 2" | 34 % |
| CVN | 120 ft.-lbs., 163 J |
| Temperature | -50 ºF, -46 ºC |
| Typical Undiluted Weld Metal Analysis | |
| As Welded | |
| Spoolarc 81 | |
| C | 0.06 % |
| Mn | 1.60 % |
| Si | 0.30 % |
| P | 0.013 % |
| S | 0.009 % |
| Spoolarc 75 | |
| C | 0.06 % |
| Mn | 1.80 % |
| Si | 0.50 % |
| P | 0.013 % |
| S | 0.009 % |
| Ni | 0.90 % |
| Spoolarc ENi4 | |
| C | 0.07 % |
| Mn | 1.60 % |
| Si | 0.20 % |
| P | 0.012 % |
| S | 0.006 % |
| Ni | 1.80 % |
| Mo | 0.15 % |
| Cu | 0.15 % |
Basicity Index: 1.9
Chemical Composition:
SiO2 + TiO2 20
Al2 + MnO 25
CaO + MgO 30
Fluorides 25
Flux Consumption
(lb. Flux / lb. Wire)
Voltage DC+
26 0.69
30 0.88
34 1.3
38 1.66