Print this page

OK Autrod 12.24

ESAB Welding & Cutting Products introduces OK Autrod 12.24, a molybdenum- alloyed, copper-coated wire for submerged arc welding of non-alloyed and low-alloyed steels.

Features

ESAB Welding & Cutting Products introduces OK Autrod 12.24, a molybdenum- alloyed, copper-coated wire for submerged arc welding of non-alloyed and low-alloyed steels. Designed for creep resistant steels (0.5% Mo), this wire is ideal for use with structural steels, ship building steels, pressure vessel steels and pipeline steels. This wire meets SFA/AWS 5.23: EA2 classification, providing superior mechanical properties to those achieved with EA1 wire. OK Autrod 12.24 in the new 2,200 lb EcoCoil™ package will provide pipe mills with high productivity, high-quality product they require. Additionally, this alloy is well-suited to the fabrication of pressure vessels that require post-weld heat treatment.

OK Autrod 12.24 - Web Image - Medium
  • Industry
  • Civil Construction
  • Shipbuilding
  • Bridge Construction
  • Pressure Vessel
  • Pipeline
  • Steel Industry

Classifications

  • Classifications/Approvals

    • AWS A5.23 EA2

Properties

Typical Properties
C 0.10 %
Mn 1.06 %
Si 0.15 %
P 0.013 %
S 0.014 %
Cr 0.04 %
Ni 0.02 %
Mo 0.50 %

SAW

Accessories

Depositions

Subarc Deposition Data
Diameter Amps Deposition Rate Efficiency %
1/8 in 400 A 11.0 lbs/hr 99
500 A 14.5 lbs/hr 99
600 A 18.0 lbs/hr 99
700 A 21.2 lbs/hr 99
5/32 in 500 A 12.5 lbs/hr 99
600 A 16.0 lbs/hr 99
700 A 19.5 lbs/hr 99
800 A 23.0 lbs/hr 99
900 A 26.0 lbs/hr 99

Extra Info

Usable with OK Flux 10.62, 10.71 and 10.72.