Print this page

Covered Electrodes - Stainless Steel

For the welder, an Arcaloy electrode deposit meets the quality control standards and produces results that he can be proud of. These premium electrodes available in a wide variety of alloys are manufactured in an ASME certified quality assurance system that insures the product meets the most rigid metallurgical, chemical and engineering solutions.

E308 (Arcaloy 308L-15)
E308 (Arcaloy 308L-15)

Arcaloy 308L-15 was developed for welding 304L stainless.

E308 (Arcaloy 308L-16)
E308 (Arcaloy 308L-16)

Arcaloy 308L-16 was developed for welding 304L stainless.

E308 (Arcaloy 308/308H-15)
E308 (Arcaloy 308/308H-15)

Arcaloy 308/308H-15 is for welding types 304H and 347H stainless when high temperature service is required.

E308 (Arcaloy 308/308H-16)
E308 (Arcaloy 308/308H-16)

Arcaloy 308/308H-16 was developed for welding types 304H and 347H stainless when high temperature service is required.

E308 (Arcaloy Plus 308L-17)
E308 (Arcaloy Plus 308L-17)

Arcaloy 308L Plus electrode utilize a heavy coating to maximize performance in the flat and horizontal position.

E309 (Arcaloy 309L-15)
E309 (Arcaloy 309L-15)

Arcaloy 309L-15 is used primarily in the overlay of steel or to join stainless steel to carbon or low alloy steels. Best used out-of-position on DC current only.

E309 (Arcaloy 309L-16)
E309 (Arcaloy 309L-16)

Arcaloy 309L-16 is used primarily in the overlay of steel or to join stainless steel to carbon or low alloy steels. Usable on AC or DC current.

E309 (Arcaloy 309MoL-15)
E309 (Arcaloy 309MoL-15)

Arcaloy 309MoL-15 is designed for applications requiring molybdenum with a standard 309L analysis. Ideal for cladding prior to joining stainless steel to low alloy steels. Best used out-of-position on DC current.

E309 (Arcaloy 309MoL-16)
E309 (Arcaloy 309MoL-16)

Arcaloy 309MoL-16 is designed for applications requiring molybdenum with a standard 309L analysis. Ideal for cladding prior to joining stainless steel to low alloy steels. Usable on AC or DC current.

E309 (Arcaloy Plus 309L-17)
E309 (Arcaloy Plus 309L-17)

Arcaloy 309L-17 Plus electrodes utilize a heavy coating to maximize performance in the flat and horizontal position. Usable on AC or DC current.

E309 (Arcaloy 309/309H-16)
E309 (Arcaloy 309/309H-16)

Arcaloy 309/309H-16 is used for welding type 309 base metal when high temperature service is required. Usable on AC or DC current.

E309 (Arcaloy 309/309H-15)
E309 (Arcaloy 309/309H-15)

Arcaloy 309/309H-15 is used for welding type 309 when high temperature service is required. Best used out-of-position on DC current.

E309 (Arcaloy 309Cb-16)
E309 (Arcaloy 309Cb-16)

Arcaloy 309Nb-16 was developed to control carbide precipitation in this type of alloy. Usable on AC or DC current.

E309 (Arcaloy 309Cb-15)
E309 (Arcaloy 309Cb-15)

Arcaloy 309Nb-15 was developed to inhibit carbide precipitation in this type of alloy. Best used out-of-position on DC current.

E310 (Arcaloy 310-15)
E310 (Arcaloy 310-15)

Arcaloy 310-15 electrodes were developed for the welding of type 310 stainless steel. Best used out-of-position on DC current.

E310 (All-State 310-16)
E310 (All-State 310-16)

Arcaloy 310-16 electrodes were developed for the welding of type 310 stainless steel. Usable on AC or DC current.

E312 (Arcaloy 312-15)
E312 (Arcaloy 312-15)

Arcaloy 312-15 electrodes were originally designed for welding of high tensile alloys to high temperature heat-resisting alloys. Best used out-of-position on AC or DC current.

E312 (All-State 312-16)
E312 (All-State 312-16)

Arcaloy 312-16 electrodes were originally designed for welding of high tensile alloys to high temperature heat-resisting alloys. Usable on AC or DC current.

E316 (Arcaloy Plus 316L-17)
E316 (Arcaloy Plus 316L-17)

Arcaloy 316L-Plus electrode utilizes a heavy coating to maximize performance in the flat and horizontal position. Usable on AC or DC current.

E316 (Arcaloy 316LF5-16)
E316 (Arcaloy 316LF5-16)

Arcaloy 316LF5-16 is an electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. Designed to weld type 316, 316L steels. Usable on AC or DC current.

E316 (Arcaloy 316LF5-15)
E316 (Arcaloy 316LF5-15)

Arcaloy 316LF5-15 is an electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. Designed to weld type 316, 316L steels. Best used out-of-position on DC current.

E316 (Arcaloy 316/316H-16)
E316 (Arcaloy 316/316H-16)

Arcaloy 316/316H-16 can be used in applications where 316 stainless needs improved due to higher service temperatures. Usable on AC or DC current.

E316 (Arcaloy 316/316H-15)
E316 (Arcaloy 316/316H-15)

Arcaloy 316/316H-15 can be used in applications where 316 stainless needs improved due to higher service temperature. Best used out-of-position on DC current.

E316 (Cryoarc 316L-15)
E316 (Cryoarc 316L-15)

Cryoarc 316L-15 is a covered electrode designed for low temperature cryogenic applications. Pre-test lot controlled formulation to maximize mechanical properties. Best used out-of-position on DC current.

E317 (Arcaloy 317L-15)
E317 (Arcaloy 317L-15)

Arcaloy 317L-15 electrodes are recommended for welding type 317 and 317L. The addition of molybdenum improves the weld metal crack resistance. Best used out-of-position on DC current.

E317 (Arcaloy 317L-16)
E317 (Arcaloy 317L-16)

Arcaloy 317L-16 electrodes are recommended for welding type 317 and 317L. The addition of molybdenum improves the weld metal crack resistance. Usable on AC or DC current.

E317 (Arcaloy Plus 317L-17)
E317 (Arcaloy Plus 317L-17)

Arcaloy 317L-17 Plus electrodes utilize a heavy coating to maximize performance in the flat and horizontal positions. Usable on AC or DC current. The addition of molybdenum improves resistance to pitting corrosion.

E320 (Arcaloy 320LR-16)
E320 (Arcaloy 320LR-16)

Arcaloy 320LR-16 is a covered electrode designed to resist hot cracking on Carpenter No.20 Cb-3 steel. Usable on AC or DC current.

E320 (Arcaloy 320-15)
E320 (Arcaloy 320-15)

Arcaloy 320-15 electrodes are designed for welding Carpenter Stainless No. 20 Cb-3. Best used out-of-position on DC current.

E347 (Arcaloy 347-16)
E347 (Arcaloy 347-16)

Arcaloy 347-16 electrodes are especially designed for welding types 347 and 321 alloys. Usable on AC or DC current.

E347 (Arcaloy 347-15)
E347 (Arcaloy 347-15)

Arcaloy 347-15 electrodes are especially designed for welding types 347 and 321 alloys. Best used out-of-position on DC current.

E410 (Arcaloy 410NiMo-16)
E410 (Arcaloy 410NiMo-16)

Arcaloy 410 NiMo-16 is designed for the welding of CA-6NM castings. Usable on AC or DC current.

E410 (Arcaloy 410-16)
E410 (Arcaloy 410-16)

Arcaloy 410-16 electrodes are recommended for welding type 410 straight chromium steel. Usable on AC or DC current.

Duplex (OK 67.50)
Duplex (OK 67.50)

ESAB OK 67.50 is an E2209-17 heavy-coated duplex covered electrode for flat & horizontal position welding. The heavy coating is designed to maximize performance on either AC or DC current.

Duplex (OK 67.55)
Duplex (OK 67.55)

OK 67.55 is an E2209-15 coated electrode specially designed for the welding of duplex stainless steel. The deposited weld metal gives very high ductility down to -45°F/-51°F. Best used out-of-position on DC current.

OK 67.45 (E307-15)
OK 67.45 (E307-15)

Suitable for joining 12 -14% manganese steel to itself or other steels. It is also suitable for buffer layers before hardfacing.

OK 61.35 (E308L-15)
OK 61.35 (E308L-15)

OK 61.35 is a basic, low-carbon, stainless electrode of the E308L type with very good welding properties in the vertical and overhead positions.

OK 61.30 (E308L-17)
OK 61.30 (E308L-17)

OK 61.30 is an extra-low carbon, AC/DC, LMA electrode for welding steel of the 19Cr10Ni type. It is also suitable for welding stabilised stainless steels of similar composition, except when the full creep resistance of the base material is to be met.

OK 67.75 (E309L-15)
OK 67.75 (E309L-15)

OK 67.75 is a basic coated, stainless electrode for welding steels of the 24Cr13Ni type, for welding transition layers when surfacing mild steel with stainless, for joining dissimilar steels and welding root runs in the stainless side of clad steels.

OK 67.60 (E309L-17)
OK 67.60 (E309L-17)

OK 67.60 is an over-alloyed, stainless electrode for welding stainless to mild steel and low-alloy steel, for surfacing mild steel and for welding the root runs in clad steel.

OK 67.70 (E309MoL-17)
OK 67.70 (E309MoL-17)

OK 67.70 is an over-alloyed, stainless-steel electrode for use as a buffer layer when welding acid resistant clad steels and stainless steels to other types of steel.

OK 68.81 (E312-17)
OK 68.81 (E312-17)

OK 68.81 is a high-alloyed electrode which deposits a ferritic-austenitic duplex weld metal with approx. 40% ferrite. It is resistant to stress corrosion and is highly insensitive to dilution.

OK 63.20 (E316L-16)
OK 63.20 (E316L-16)

OK 63.20 is a rutile electrode with an extra-low carbon content for welding stainless steel of the 316L, 18Cr12Ni3Mo type. The electrode is specially designed for the positional welding of thin walled pipes.

OK 63.34 (E316L-16)
OK 63.34 (E316L-16)

OK 63.34 is a stainless electrode of the 19Cr12Ni2.8Mo type, designed for the vertical-down welding of steels of similar composition

OK 63.30 (E316L-17)
OK 63.30 (E316L-17)

OK 63.30 is an extra-low carbon, LMA electrode of the 18Cr12Ni2.8Mo type. It is also suitable for welding stabilised steels of similar composition, except when the full creep resistance of the base material has to be met.

OK 63.41 (E316L-26)
OK 63.41 (E316L-26)

OK 63.41 is an extra-low carbon, acid-resistant, high-recovery LMA electrode of the 18Cr12.5Ni2.8Mo type. The electrode is intended for use in the flat position and produces smooth,shiny beads.

OK 64.30 (E317L-17)
OK 64.30 (E317L-17)

OK 64.30 is an acid-rutile electrode for welding 19Cr 13Ni 3.5Mo (317L) austenitic stainless steels. The high Mo content provides better resistance to acid and pitting corrosion compared with 316L types.

OK 61.81 (E347-16)
OK 61.81 (E347-16)

OK 61.81 is a niobium-stabilised, stainless welding electrode for titanium- and niobium-stabilised 18-8 steel. It is particularly suitable for high temperature applications.

OK 61.80 (E347-17)
OK 61.80 (E347-17)

OK 61.80 is a niobium-stabilised, stainless-steel, LMA electrode with low carbon content for welding stainless types 321 and 347.

OK 69.33 (E385-16)
OK 69.33 (E385-16)

OK 69.33 is a stainless-steel electrode which deposits a fully austenitic weld metal with increased resistance to sulphuric acid.

OK 68.15 (E410-15)
OK 68.15 (E410-15)

OK 68.15 is a stainless-steel electrode which deposits a ferritic 13Cr weld metal. OK 68.15 is designed for welding steels of similar composition, when CrNi-alloyed austenitic stainless steel electrodes cannot be used, e.g. when the structure is going to be exposed to aggressive sulphuric gases.

OK 68.17 (E410NiMo-16)
OK 68.17 (E410NiMo-16)

OK 68.17 is a coated electrode designed for the welding of stainless-steel castings of the 13Cr4NiMo type, for example. OK 68.17 can be welded in all positions apart from vertical down.

OK 68.55 (Super Duplex type)
OK 68.55 (Super Duplex type)

OK 68.55 is a basic coated electrode for welding austenitc-ferritic steels of the Super Duplex type, e. g. SAF 2507 and Zeron 100. OK 68.55 deposits a weld metal with high ductility.