Covered Electrodes - Cast Iron

Nickel-Arc covered electrodes are specially formulated for welding and repair of cast iron materials. The arc characteristics optimize the maximum efficiency while providing the user with the utmost quality and reliability.

Nickel-Arc 550 (ENiFE-CI-A)
Nickel-Arc 550 (ENiFE-CI-A)

Nickel-Arc 550 was developed as a new and improved Nickel-Arc 55. The primary advantage of this electrode is its superior resistance to over-heating, thus producing maximum deposition efficiency and maximum utilization.

Nickel-Arc 55 (ENiFE-CI-A)
Nickel-Arc 55 (ENiFE-CI-A)

Nickel-Arc 55 is designed for welding nodular cast iron to steel. This electrode's deposit is sound, crack-free and produces good color matching on gray malleable or nodular cast iron.

Nickel-Arc 99 (ENiCI-A)
Nickel-Arc 99 (ENiCI-A)

Nickel-Arc 99 is designed for welding gray, malleable and nodular cast iron. It uses pure nickel core wire for applications requiring high nickel deposit.

OK 92.18 (ENi-Cl)
OK 92.18 (ENi-Cl)

A nickel-cored electrode for welding normal grades of cast iron. The weld metal is soft and easily machinable.

OK 92.58 (ENiFe-Cl)
OK 92.58 (ENiFe-Cl)

A nickel-iron-cored electrode for joining normal grades of cast iron, such as grey, ductile and malleable irons. It is also suitable for the rectification and repair of these grades and for joining them to steel.