Covered Electrodes - Hard Surfacing

Wear-Arc covered electrodes are uniquely designed for hard-surfacing and build-up. These electrodes provide maximum resistance to specific destructive wear factors such as abrasion, compression, deformation, heat or corrosion.

Wear-Arc Ni-Mn (EFeMn-A)
Wear-Arc Ni-Mn (EFeMn-A)

Wear-Arc Ni-Manganese is a "build-up" alloy that produces a crack resistant weld deposit that forms a ductile, hig strength bond.

Wear-Arc 3-IP (No AWS Class)
Wear-Arc 3-IP (No AWS Class)

Wear-Arc 3-IP weld metal provides excellent resistance to wear caused by heavy impact and compressive loads.

Wear-Arc 4-IP (No AWS Class)
Wear-Arc 4-IP (No AWS Class)

Wear-Arc 4-IP is a covered electrode hardsurfacing alloy for metal to metal wear and moderate impact and abrasion.

Wear-Arc 5-IP (No AWS Class)
Wear-Arc 5-IP (No AWS Class)

Wear-Arc 5-IP is a covered electrode hardsurfacing alloy for high impact and moderate abrasion.

Wear-Arc 6-IP (No AWS Class)
Wear-Arc 6-IP (No AWS Class)

The iron powder low hydrogen coating of Wear-Arc 6-IP electrodes promotes good bonds with manganese and carbon steels.

Wear-Arc 12-IP (No AWS Class)
Wear-Arc 12-IP (No AWS Class)

Wear-Arc 12-IP is a hardsurfacing covered electrode for heavy impact and good abrasion.

Wear-Arc 40 (No AWS Class)
Wear-Arc 40 (No AWS Class)

Wear-Arc 40 is a coated electrode with a special core wire and the proper amount of alloys in the coating to produce a deposit of highly abrasive resistant chrome carbides in a matrix of iron and chromium.

Wear-Arc WH (No AWS Class)
Wear-Arc WH (No AWS Class)

The weld deposit of Wear-Arc WH is high in alloy content, extremely deformation resistant, and has 2-4 times greater wear resistance than work-hardened austenitic manganese steel.