Print this page

Solid Wire - Stainless Steel

Arcaloy bare stainless steel spools, coils and cut lengths are manufactured under a carefully administered, high standard quality control program developed through years of experience in welding wire production. Temper, cast, helix and surface finish are closely controlled, as the uniformity of these properties is essential to the maximum efficiency of your weld.

OK Autrod 308L (ER308/308L)
OK Autrod 308L (ER308/308L)

OK Autrod 308L is a low carbon MIG wire and has good general corrosion resistance.

OK Autrod 309L (ER309/309L)
OK Autrod 309L (ER309/309L)

OK Autrod 309L is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding of similar steels, wrought and cast steels of 23% Cr - 12% Ni types.

OK Autrod 2209 (ER2209)
OK Autrod 2209 (ER2209)

OK Autrod 2209 is a duplex stainless steel for welding type 2205 duplex stainless.

OK Autrod 2509 (No AWS Class)
OK Autrod 2509 (No AWS Class)

OK Tigrod 2509 is a super duplex grade for high resistance to intergranular corrosion and pitting. The alloy is widely used in applications in which corrosion resistance is of the utmost importance. Can be used in combination with OK Flux 10.94.

OK Tigrod 316L (ER316/316L)
OK Tigrod 316L (ER316/316L)

OK Tigrod 316L has good general corrosion resistance, particularly to corrosion in acid and chlorinated environments. This alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion.

OK Tigrod 309L (ER309/309L)
OK Tigrod 309L (ER309/309L)

OK Tigrod 309L is used for welding buffer layers on CMn steels and for welding dissimilar joints. When using the wire for buffer layers and dissimilar joints, it is necessary to control the dilution of the weld.

OK Autrod 309LSi (ER309Si/309LSi)
OK Autrod 309LSi (ER309Si/309LSi)

OK Autrod 309LSi has good general corrosion resistance. This high silicon MIG wire improves the wetting characteristics of the weld deposit.

OK Tigrod 308L (ER308/308L)
OK Tigrod 308L (ER308/308L)

OK Tigrod 308L is a bare, corrosion-resistant, chromium-nickel TIG rod. OK Tigrod 308L has a good general corrosion resistance. The alloy has a low carbon content which makes this alloy particularly recommended where there is a risk of intergranular corrosion.

OK Autrod 308LSi (ER308Si/308LSi)
OK Autrod 308LSi (ER308Si/308LSi)

OK Autrod 308LSi has good general corrosion resistance. This high silicon MIG wire improves wetting characteristics of the weld deposit.

OK Autrod 16.95 (307Si, No AWS Class)
OK Autrod 16.95 (307Si, No AWS Class)

OK Autrod 16.95 (307Si) is a high silicon MIG wire that improves wetting characteristics of the weld deposit. This alloy is used for joining of austenitic, manganese, work-hardenable steels, as well as armour plate and heat-resistant steels.