All Spoolarc Mig wires are cleaned after the final drawing process and then treated with a proprietary process to ensure good feedability, arc stability and low weld deposit hydrogen. Excellent arc characteristics provide precise control of the welding process with better current transfer for longer contact tip life.
Spoolarc Easy Grind is a fully deoxidized wire designed to weld over the moderate levels of rust and paint commonly encountered in auto body repair work.
Spoolarc 65 is a triple deoxidize (Aluminum, Titanium, Zirconium) GMAW/GTAW welding wire. It's sluggish puddle makes it suitable for out of position welding. Spoolarc 65 produces extremely good impact properties using the GTAW process.
Spoolarc 29S is a general purpose wire suitable for many MIG and submerged arc carbon steel welding applications. Suitable for use over light rust.
Spoolarc 82 is a premium quality wire suitable for many general purpose carbon steel MIG welding applications. Spoolarc 82 is suitable for use over light rust.
Spoolarc 85 contains moderate levels of deoxidizers and is suitable for many general purpose carbon steel MIG applications. Spoolarc 85 can be used over light rust or light mill scale.
Spoolarc 86 contains higher levels of manganese and silicon than other grades of MIG wire. It provides a highly fluid puddle and excellent tolerance of rust and scale.
Spoolarc 87 HP features an optimized manganese to silicon ratio. It is suitable for welding over moderate amounts of rust and scale.