Print this page

Gas-Shielded Flux Core

Shield-Bright wires were specially developed for out-of-position welding and will deposit out-of-position welds at substantially higher welding currents than other stainless steel electrodes, for high deposition and maximum productivity. A self-peeling slag minimizes clean up.

Cryo-Shield 308L (E308LT1)
Cryo-Shield 308L (E308LT1)

Cryo-Shield 308L is an all-position stainless steel cored wire designed for low temperature cryogenic applications.

Shield-Bright 308L X-tra (E308LT0)
Shield-Bright 308L X-tra (E308LT0)

Shield-Bright 308L X-tra was developed to maximize performance in the flat and horizontal position on type 304 or 304L steels.

Shield-Bright 308L (E308LT1)
Shield-Bright 308L (E308LT1)

Shield-Bright 308L was developed for out-of-position welding on type 304 or 304L steels.

Shield-Bright 308H (E308HT1)
Shield-Bright 308H (E308HT1)

Shield-Bright 308H was developed for out-of-position welding on type 304H or 347H steels where high temperature service is required.

Shield-Bright 309LMo X-tra (E309LMoLT0)
Shield-Bright 309LMo X-tra (E309LMoLT0)

Shield-Bright 309LMo X-tra was developed to maximize performance in the flat and horizontal positions when joining or cladding stainless to low alloy steels.

Shield-Bright 309L X-tra (E309LT0)
Shield-Bright 309L X-tra (E309LT0)

Shield-Bright 309L X-tra was developed to maximize performance in the flat and horizontal positions when joining stainless to mild or carbon steel.

Shield-Bright 309LMo (E309LMoT1)
Shield-Bright 309LMo (E309LMoT1)

Shield-Bright 309LMo was developed as an over-alloyed wire used in cladding and joining dissimilar metals.

Shield-Bright 309L (E309LT1)
Shield-Bright 309L (E309LT1)

Shield-Bright 309L was developed for out-of-position welding when joining stainless to mild or carbon steel.

Shield-Bright 309H (E309LT1)
Shield-Bright 309H (E309LT1)

Shield-Bright 309H was developed for out-of-position weld on 309H stainless where high temperature service is required.

Shield-Bright 312 (E312T1)
Shield-Bright 312 (E312T1)

Shield-Bright 312 was developed for out-of-position welding when joining stainless to high carbon and low alloy steels.

Shield-Bright 316L X-tra (E316LT0)
Shield-Bright 316L X-tra (E316LT0)

Shield-Bright 316L X-tra was developed to maximize performance in the flat and horizontal positions when improved corrosion resistance is needed on 316 and 316L steels.

Shield-Bright 316L (E316LT1)
Shield-Bright 316L (E316LT1)

Shield-Bright 316L was developed for out-of-position welding when improved corrosion resistance is needed on 316 and 316L steels.

Shield-Bright 316H (E316T1)
Shield-Bright 316H (E316T1)

Shield-Bright 316H was developed for out-of-position welding when required in high temperature service when using 316 steel.

Shield-Bright 317L X-tra (E317LT0)
Shield-Bright 317L X-tra (E317LT0)

Shield-Bright 317L X-tra was developed to maximize performance in the flat and horizontal position when the addition of molybdenum improves corrosion resistance.

Shield-Bright 317L (E317LT1)
Shield-Bright 317L (E317LT1)

Shield-Bright 317 was developed for out-of-position welding when the addition of Molybdenum improves corrosion resistance.

Shield-Bright 347H (E347T1)
Shield-Bright 347H (E347T1)

Shield-Bright 347H was developed for out-of-position welding when required in high temperature service on type 347.

Shield-Bright 347 (E347T1)
Shield-Bright 347 (E347T1)

Shield-Bright 347 was developed for out-of-position welding on types 347, 304, 304L, and 321 steels.

Shield-Bright 2509 (No AWS Class)
Shield-Bright 2509 (No AWS Class)

Shield-Bright 2509 is a "super duplex" stainless flux cored wire developed for out-of-position welding on 2507 or similar super duplex steels.

Shield-Bright 2209 (E2209T1)
Shield-Bright 2209 (E2209T1)

Shield-Bright 2209 is a "duplex" stainless flux cored wire developed for out-of-position welding on 2209 or similar duplex steels.