A self-fluxing brazing alloy for copper to copper joining. Use for higher ductility in joints where close fit-up is impossible (.002" to .006") and electrical conductivity is important. Do not use with ferrous metals. For best result use with All-State S-200 or No.110 when joining copper to brass or bronze.
A self-fluxing brazing alloy for copper to copper (.001" to .002"). Do not use with ferrous metals. For best results use with All-State S-200 or No. 110 flux when joining copper to brass or bronze.
A self-fluxing brazing alloy for copper to copper joining. For tight fitting joints (.001" to .002"). Do not use with ferrous metals. For best results use with All-State S-200 or No. 110 flux when joining copper to brass or bronze.
A premium general purpose, flux coated bronze rod for joining or overlaying of steel, cast iron, brass, bronze, galvanized and malleable irons or any combination of these metals. Excellent for hobbyists and artists.
A welding wire that produces high purity deposits for fabricating deoxidized copper. Also used to join copper to steel or overlay them. Provides high electrical conductivity and excellent corrosion resistance. Use with 100% Ar or 25/75 Ar/He shielding gas.
A welding wire for fabricating and joining silicon bronze, copper alloys, some iron-base metals and thin gauge galvanized steel. Deposits are high strength, ductile and crack resistant. Especially good on galvanized steel. Use with 100% Ar or 25/75 Ar/He shielding gas.
A general purpose brazing rod for fabricating or repairing steels, cast iron, copper base metals, galvanized and malleable irons or any combination of these metals. Available as base or build-up repair.
An electrode that produces sound, porosity-free welds on bronze, cast-iron, steel and some brass and copper alloys (non-lead) as well as to each other. The higher the copper content of the part, the higher the required pre-heat.
An electrode of welding aluminum bronze, manganese bronze, silicon bronze and bronze to steel, cast iron and other ferrous alloys. Deposits are strong, dense, ductile, crack free and have good resistance to corrosion caused by salt water and many acids and alkalis.