Oxweld Acetylene Nozzles - 1516 Series
Acetylene nozzle for cutting and trimming.
- Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
- One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
- Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
- Long, parallel preheat passages – permit re-dressing nozzle without affecting performance
- One-piece nozzle is a single piece of solid copper – provides maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
- Two-piece nozzles – recommended for high efficiency with fuel gases other than acetylene – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost
- Conical seats – instant aligning provides tight seal, prevents leaks around nozzle nut
1516 Series
| Metal Thickness |
3/4-1-1/2 in., 19-38 mm |
| Nozzle Size |
6 in. |
| No. Preheat Holes or Slots |
4 |
| Gas Pressure |
|
| Cutting Oxygen |
35-40 PSIG |
| Cutting Acetylene |
5-7 PSIG |
| Gas Consumption |
|
| Total Oxygen |
120-150 CFH |
| Acetylene |
15-20 CFH |
1516 Series
| 65Z22 |
1516 NOZZLE #6 |
662067017874 |
| There are no accessories. |