Print this page

Purox Hand or Machine Cutting Aceytlene Nozzles - 4202 Series

General purpose. Medium preheat sufficient for beveling.

Features

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages – permit re-dressing nozzle without affecting performance
  • One-piece nozzle is a single piece of solid copper – provides maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece nozzles – recommended for high efficiency with fuel gases other than acetylene – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost
  • Conical seats – instant aligning provides tight seal, prevents leaks around nozzle nut

Classifications

Specifications

4202 Series
Metal Thickness 1/8 to 12 in., 3-300 mm
Nozzle Size 1/8-12
No. Preheat Holes or Slots 4-6
Cleaning Preheat 56-73
Drill Size Cutting 30-76
Gas Pressure  
Cutting Oxygen 15 to 85 PSIG
Cutting Acetylene 5 to 12 PSIG
Cutting Speed 1 to 40 ipm
Gas Consumption  
Total Oxygen 20-860 CFH
Acetylene 5-52 CFH
Average Kerf Width .050-.210 in.

Ordering

Configure this Model

Part No.

4202 Series
Part No. Model / Product Description UPC
Q4202-11 4202-11 PUROX STL TIP 10 IN 662067159321
Q4202-3 4202-3 PUROX STL TIP 1/4 IN 662067159338
Q4202-4 4202-4 PUROX STL TIP 1/2 IN 662067159345
Q4202-5 4202-5 PUROX STL TIP 662067159352
Q4202-7 4202-7 PUROX STL TIP 4 IN 662067159369
Q4202-9 4202-9 PUROX STL TIP 6 IN 662067159376
16K08 4202 NOZZLE 1/4 IN 662067016457
16K12 4202 NOZZLE 6 IN 662067016495
16K13 4202 NOZZLE 10 IN 662067016501
16K14 4202 NOZZLE 12 IN 662067016518
638869 4202 NOZZLE 1/8 IN 662067016648

Accessories

There are no accessories.

Package Contents