ESAB welding torches are constructed with pressure-forged brass in the rear body to provide an excellent strength-to-weight ratio, silver-brazed joints for high rigidity and resistance to gas leakage, and swaged copper tips for maximum heat and wear resistance. Separate heavy-walled seamless brass tubes minimize the possibility of gases mixing within the handle and an exclusive coiled oxygen tube resists flashbacks.

ESAB's Gas Apparatus Lifetime Warranty applies to Oxweld®, Purox® and Prest-O-Lite® standard torches, regulators and flowmeters and covers manufacturer defect in materials and workmanship as well as normal wear and tear.