Print this page

Acetylene Nozzles

1502 Series
1502 Series

General Purpose. Medium Preheat, sufficient preheat for cutting dirty plate and for beveling.

1507 Series
1507 Series

Unsurpassed for washing off rivet heads and then piercing rivet to facilitate removal. Each nozzle is equipped with a spud which produces a low-velocity oxygen-stream.

1510 Series
1510 Series

For riser removal. Except in length, comparable to 1502. Supplied straight, with instructions for bending.

1511 Series
1511 Series

Acetylene nozzle for gouging, grooving plate edges for welding, removing defects from castings, pad washing. Bent 20 degrees. 1511 nozzles have wear stellite skids

1514 Series
1514 Series

Acetylene nozles for high speed cutting. Medium preheat sufficient for beveling.

1516 Series
1516 Series

Acetylene nozzle for cutting and trimming.

1563 Series
1563 Series

High speed with low acetylene consumption. Divergent Bore Cutting Oxygen Hole.

1564 Series
1564 Series

To clean preheat slots, remove external sleeve and use a soft bristled brush. Use where high preheat intensity is desired.

1565 Series
1565 Series

Low acetylene consumption (7 to 30 chf). Sufficient preheat for beveling clean plate up to 45 deg.

4202 Series
4202 Series

Hand or Machine cutting acetylene nozzle for general purpose use. Medium preheat sufficient for beveling.

4206 Series
4206 Series

Light preheat for cutting sheet metal.

4207 Series
4207 Series

Designed for grooving, gouging and plate edge preparation.

4209 Series
4209 Series

Designed for rivet busting and bolt removal.

SABRE "V" Oxy-Acetylene Cutting Nozzle

The newest Sabre “V” series features top quality oxy-fuel equipment. Interchangeable with Uniweld® and Turbotorch®.