SD 5

Self-aligning Rollerbeds, 2.5 metric ton load capacity.

Features

  • Robust design with durable rollers
  • Gritblasted steelwork with polyurethane finished coating to endure the abrasive environments
  • Over-sized bearings
  • Specially formulated high-load polyurethane tire design for high wear resistance
  • Cast steel gearbox with double worm gear arrangement for smooth operation and minimum backlash
  • Solid-state inverter for precise speed control
  • Motorized and Idler Rail Bogie versions available

Classifications

Specifications

SD 5
Max load 2.5 metric ton, 2.8 US ton
Rolling Capacity 5 metric ton
Rotation speed 100-1000 mm/min, 4-39 ipm
Diameter range min-max 250-2300 mm, 10-90.5 in
Length  
Power 1900 mm, 75 in
Idler 1160 mm, 45.6 in
Width  
Power 660 mm, 26 in
Idler 400 mm, 15.7 in
Weight  
Power 700 kg, 1543 lb
Idler 300 kg, 661 lb
Primary Input Voltage, VAC, 60 Hz 415 3ph
Primary Input Current 16 A

Ordering Information

Configure this Model

Part No.

SD 5
Part No. Model / Product Description UPC
370250064 SD-5-DB Drive Unit with Motorized Rail Bogie  
370250050 DRIVE UNIT SD 5  
370250051 SI 5 IDLER UNIT  

Accessories

There are no accessories.

Extra Info