Print this page

Spoolarc 81

Spoolarc 81 is a medium manganese and silicon wire with nominal rust and mill scale tolerance. Typical applications include structural steels, medium strength pressure vessels, ship, barge, and offshore oil rig fabrication.

Features

Medium manganese and silicon wire - nominal rust and mill scale tolerance.
Developed for general purpose welding on low and medium carbon steels.
Applications include structural steels, medium strength pressure vessels, ship, barge and offshore oil rig fabrication.
Use with OK Flux 50, 80, 429, 231, 350, 10.71, 10.72, and 10.62 fluxes.

Spoolarc 81
  • Welding Process
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • AWS A5.17; EM12K

Properties

Typical Properties
C 0.1 %
Mn 1.0 %
Si 0.2 %
P 0.008 %
S 0.010 %
Typical wire analysis  
C 0.11 %
Mn 0.95 %
Si 0.26 %
P 0.006 %
S 0.008 %

Part No.

81
Part No. Model / Product Description UPC
120KF90 81 3/32X1000#RL-3 VERT/PLT 662303080563
120UF48 81 1/16X900#OMP 2/PLT 662303668860
1204F28 81 1/16X65#CL 662303503727
1204F29 81 5/64X65#CL 662303503734
1204F30 81 3/32X65#CL 662303503741
1204F32 81 1/8X65#CL 662303503758
1204F34 81 5/32X65#CL 662303503765
1204F35 81 3/16X65#CL 662303503772
1205F30 81 3/32X200#CL 662303522780
1205F34 81 5/32X200#CL 662303517588
1206F09 81 5/64X800#DR 662303503796
1206F10 81 3/32X800#DR 662303503802
1206F12 81 1/8X800#DR 662303503819
1206F14 81 5/32X800#DR 662303503826
1206F15 81 3/16X800#DR 662303503833
1206F34 81 5/32X300#DR 662303503857
1206F49 81 5/64X700#DR 662303503871
1206F50 81 3/32X700#DR 662303503888
1206F52 81 1/8X700#DR 662303503895
1206F54 81 5/32X700#DR 662303503901
1206F55 81 3/16X700#DR 662303503918
1208F68 81 1/16X700#RL 662303503963
1208F69 81 5/64X700#RL 662303503970
1208F72 81 1/8X700#RL 662303503994
1208F74 81 5/32X700#RL 662303504007
1208F75 81 3/16X700#RL 662303504014
1208F90 81 3/32X300#RL 013603 RL 662303668501
1209F48 81 1/16X900#MP PBPLT 662303518356
120EFFM 81 5/64X600#DR 16IN CORE 662303519476

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Amps Deposition Rate Average Deposition Efficiency
1/16 in, 1.6 mm 400 13.0 lbs./hr., 5.90 kg./hr. 99 %
500 17.0 lbs./hr., 7.71 kg./hr. 99 %
5/64 in, 2.0 mm 300 10.8 lbs./hr., 4.90 kg./hr. 99 %
400 14.5 lbs./hr., 6.58 kg./hr. 99 %
500 18.2 lbs./hr., 8.26 kg./hr. 99 %
3/32 in, 2.4 mm 400 13.2 lbs./hr., 5.99 kg./hr. 99 %
500 17.0 lbs./hr., 7.71 kg./hr. 99 %
600 22.0 lbs./hr., 9.98 kg./hr. 99 %
1/8 in, 3.2 mm 400 11.0 lbs./hr., 4.99 kg./hr. 99 %
500 14.5 lbs./hr., 6.58 kg./hr. 99 %
600 18.0 lbs./hr., 8.16 kg./hr. 99 %
700 21.2 lbs./hr., 9.62 kg./hr. 99 %
5/32 in, 4.0 mm 500 12.5 lbs./hr., 5.67 kg./hr. 99 %
600 16.0 lbs./hr., 7.26 kg./hr. 99 %
700 19.5 lbs./hr., 8.85 kg./hr. 99 %
800 23.0 lbs./hr., 10.43 kg./hr. 99 %
900 26.0 lbs./hr., 11.79 kg./hr. 99 %
3/16 in, 4.8 mm 600 13.9 lbs./hr., 6.31 kg./hr. 99 %
700 17.5 lbs./hr., 7.94 kg./hr. 99 %
800 21.0 lbs./hr., 9.53 kg./hr. 99 %
900 25.0 lbs./hr., 11.34 kg./hr. 99 %
1000 29.2 lbs./hr., 13.25 kg./hr. 99 %
1100 34.0 lbs./hr., 15.42 kg./hr. 99 %
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 150 ipm, 381 cm/min 45 14 1 lbs./hr., 0.4 kg./hr.
200 ipm, 508 cm/min 55 14 1.3 lbs./hr., 0.6 kg./hr.
250 ipm, 635 cm/min 65 15 1.6 lbs./hr., 0.7 kg./hr.
300 ipm, 762 cm/min 74 15 2 lbs./hr., 0.9 kg./hr.
350 ipm, 889 cm/min 84 16 2.3 lbs./hr., 1 kg./hr.
380 ipm, 965 cm/min 90 16 2.5 lbs./hr., 1.1 kg./hr.
.030 in, 0.8 mm 150 ipm, 381 cm/min 60 14 1.7 lbs./hr., 0.8 kg./hr.
200 ipm, 508 cm/min 80 15 2.2 lbs./hr., 1 kg./hr.
250 ipm, 635 cm/min 100 15 2.8 lbs./hr., 1.3 kg./hr.
300 ipm, 762 cm/min 120 16 3.3 lbs./hr., 1.5 kg./hr.
350 ipm, 889 cm/min 140 16 3.9 lbs./hr., 1.8 kg./hr.
360 ipm, 914 cm/min 144 16 4 lbs./hr., 1.8 kg./hr.
.035 in, 0.9 mm 180 ipm, 457 cm/min 90 15 2.7 lbs./hr., 1.2 kg./hr.
220 ipm, 559 cm/min 113 16 3.3 lbs./hr., 1.5 kg./hr.
260 ipm, 660 cm/min 137 18 4 lbs./hr., 1.8 kg./hr.
300 ipm, 762 cm/min 160 19 4.6 lbs./hr., 2.1 kg./hr.
.045 in, 1.2 mm 125 ipm, 318 cm/min 130 17 3.1 lbs./hr., 1.4 kg./hr.
160 ipm, 406 cm/min 163 18 4 lbs./hr., 1.8 kg./hr.
200 ipm, 508 cm/min 200 19 5 lbs./hr., 2.3 kg./hr.
.052 in, 1.3 mm 135 ipm, 343 cm/min 150 17 4.5 lbs./hr., 2.1 kg./hr.
190 ipm, 483 cm/min 200 20 6.4 lbs./hr., 2.9 kg./hr.
160 ipm, 406 cm/min 173 18 5.4 lbs./hr., 2.4 kg./hr.

Extra Info