Print this page

OK Flux 10.05

OK Flux 10.05 is an agglomerated flux for SAW (submerged arc) strip cladding. It is recommended for cladding with austenitic types of strip.

Features

It is recommended for cladding with Cr, CrNi, and CrNiMo types of stainless strips. The slag removal and overlapping with this flux are excellent.

OK Band 309L and OK Flux 10.05 provide a buffer layer when used with 308L, 316L, 317L, or 347 to produce the desired analysis on the second layer.

OK Flux 10.05
  • Industry
  • Petrochemical
  • Process
  • Welding Process
  • SAW (Sub Arc)

Classifications

Properties

Typical Properties
OK Flux 10.05  
Typical Undiluted Weld Analysis, As Welded  
1st layer welded with OK Band 309L  
OK Band 308L  
C 0.02 %
Mn 1.10 %
Si 0.60 %
Cr 18.5 %
Ni 10.40 %
Mo 0.06 %
OK Band 316L  
C 0.02 %
Mn 1.10 %
Si 0.70 %
Cr 17.5 %
Ni 13.00 %
Mo 2.80 %
OK Band 347  
C 0.02 %
Mn 1.10 %
Si 0.70 %
Cr 19.2 %
Ni 10.30 %
Nb 0.350 %

Part No.

Flux 10.05
Part No. Model / Product Description UPC
1005100000 OK FLUX 10.05 20KG BG 662303070588
100510000A OK FLUX 10.05 20KG BG 662303076955

SAW

Accessories

Depositions/Paramaters

Extra Info

Basicity Index: 1.1

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.