OK Flux 10.94 is basic chromium alloying flux suitable for welding stainless and super duplex steels.
OK Flux 10.94 is a basic Cr alloying flux from butt welding stainless steels. OK flux 10.94 is suitable for welding stainless, high alloyed Cr Ni Mo steels like super duplex types.

| Ok Flux 10.94 | |
|---|---|
| Typical Mechanical Properties, As Welded | |
| OK Autrod 2509 | |
| Tensile Strength | 113 ksi, 780 MPa |
| Yield Strength | 91 ksi, 630 MPa |
| CVN | 66 ft-lbs, 90 J |
| Temperature | 68 °F, 20 °C |
| CVN | 37 ft-lbs, 50 J |
| Temperature | -76 °F, -60 °C |
| Typical Undiluted Weld Metal Analysis, As Welded | |
| OK Autrod 2509 | |
| C | 0.04 % |
| Si | 0.50 % |
| Mn | 0.50 % |
| Cr | 25.0 % |
| Ni | 9.50 % |
| N | 0.20 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 1094000000 | OK FLUX 10.94 25KG BG | 662303071929 |
| 109400000A | OK FLUX 10.94 25KG BG | 662303077570 |
| Basicity Index: | 1.7 |
| Chemical Composition: | |
| SiO2 + TiO2 | 10 |
| Al2 + MnO | 35 |
| Fluorides | 50 |
| Flux Consumption | |
| (lb. Flux / lb. Wire) | |
| Voltage | DC+ |
| 26 | 0.5 |
| 30 | 0.6 |
| 34 | 0.8 |
| 38 | 1.0 |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.