PowerCut® 1250 Plasmarc™ Cutting Package

The PowerCut® 1250 plasma cutting package combines the proven reliability of ESAB Plasmarc™ technology with the newly designed PT-32EH patented torch. The very strong composite case material makes the PowerCut® 1250 an excellent addition to any equipment rental fleet. The PT-32EH plasma cutting torch provides increased performance and longer consumable life, resulting in higher production rates at lower costs. It cuts up to 1-1/4 in. (32 mm).

Features

  • Cuts 1-1/4 in. manually, 5/8 in. mechanized.
  • Multi input voltage (208) 230/460V, easily changed on back of machine. Other voltages also available.
  • Designed for rugged treatment and outdoor use makes the PowerCut® an excellent choice for rental fleet and construction site uses.
  • Excellent gouging performance.
  • Self protectant against improper input voltage.
  • Multiple troubleshooting lights on front panel.
  • Built in line conditioner —handles poor power lines.
  • Arrives ready to cut, with torch connected and frontend parts in place, for the ultimate in operator convenience.
  • Three-year warranty on console.
  • One-year warranty on torch.

Classifications

Specifications

PowerCut® 1250 Plasmarc™ Cutting Package
Cuts 1-1/4 in, 32 mm
Severs 1-1/2 in, 38 mm
Output  
60% Duty Cycle 70 A, 1 ph
100% Duty Cycle 70 A, 1 ph
Input  
1 ph 208/230 vac, 50/60 Hz, 66/61 A
3 ph 208/230 vac, 50/60 Hz, 32/29 A
3 ph 230/460 vac, 50/60 Hz, 29/20 A
3 ph 400 vac, 50/60 Hz, 18 A
3 ph 575 vac, 50/60 Hz, 14 A
Dimensions  
Length 32 in, 813 mm
Width 12.5 in, 318 mm
Height 16.5 in, 419 mm
Weight 86 lbs, 39 kg
Air Requirements 350 cfh @ 80 psig, 165 l/min @ 4.8 - 5.2 bars

Ordering Information

Configure this Model

Part No.

PowerCut® 1250 Plasmarc™ Cutting Package
Part No. Model / Product Description UPC
0558003509 PC-1250 25'PKG W/TORCH WRAP  
0558004189 PC1250 MECH 208/230/460 CONS  
0558004190 PC1250 MECH 400V CE CONSOLE  
0558001933 PC-1250, 208-230/460V, 25'PT32 662067171125
0558001934 PC-1250, 200/230/460V, 50' 662067171132

Accessories

Part No. Model / Product Description List Price
0558003560 KIT SP PTS PT-32 LHS/PC-1250 $135.19
0558003508 KIT SP PTS PT-32/PC-1250 $150.60
19765 PLASMA GAS MEAS KT $443.17
0558003258 CIRCLE CUTTING KIT DELUXE $280.87
0558002675 TOR GUIDE KIT PT23/27/31/32/34 $91.79
0558003612 REMOTE HAND SWITCH PT-21AMX $134.00
0558002393 GUIDE, STAND-OFF PT-32 $18.67
0558002908 NOZZLE 40A (5) $5.53
0558003060 WHEEL CART KIT PC 1500 $163.34
0558003059 TORCH WRAP/KIT PC-1250/1500 $122.43
0558003089 NOZZLE GOUGING PT-32 (5) $10.75
0558003090 HEAT SHIELD GOUGING PT-32 $19.59
0558003374 DRAG HEAT SHIELD PT-32 $33.40
0558004206 DRAG HEAT SHIELD HVY DUTY PT32 $44.37
0558004215 CNC CABLE 50' $107.00
XWPC1250 PC1250 Extended Warranty 5yrs Call ESAB for pricing

Extra Info

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.